| Application PulsPlasma®-Nitriding | ||
![]() |
Part : | Adapter |
| Material : | 42 CrMo 4V (DIN 1.7225) | |
| Task : | improvement of wear resistance | |
| Treatment : | PulsPlasma®-Nitriding | |
| Result : | Surface hardness > 700 HV nitriding depth 0,2 mm | |
| Notes : | customer demands a tolerance of max. 0,2 mm after treatment PulsPlasma®-Nitriding at low (< 500°C) temperatures | |